+91 7359010444

Butyl Reclaimed Rubber





• Only PCR/ TBR / OTR tubes are used for the production of butyl reclaim rubber, hence it
imports excellent dimensional stability to the extruded inner-tube & imparts be with no
considerable increase in the air permeability of the final inner-tube with no reduction in
hot air aging properties.
• Excellent process ability & improved extrusion rate of the compound incorporating butyl
reclaim rubber.



Parameter
   Acetone Extract ASH Contain Carbon Black  Rubber Hydrocarbon  Moisture Elongation at break Hardness **Mooney Viscosity ML  Specific Gravity Tensile Strength
Unit % % % % % % - - - Kg./Cm2
Standard Specification
  6-12 2-6 28-36 50 Min. 1 Max 475 Min 50-60 35-50 1.14 Max 75 Min